Experts in Manufacturing Quality Investment Castings in a Range of Superalloys.

InInconel Investment Casting

Experts in Manufacturing Quality Investment Castings in a Range of Superalloys.

Superalloy Investment Casting

High Temperature Alloy & Nickel & Cobalt Investment Casting

Lestercast manufacture quality investment castings in superalloys, also known as high temperature alloys or specialist alloys.

As a reputable metal casting company, we manufacture high quality superalloy investment castings for a wide range of industries across the world. Nickel-based superalloys have high strength and long fatigue life combined with good resistance to oxidation and corrosion at high temperature. Some nickel-based superalloys can withstand temperatures beyond 1200°C, depending on the composition of the alloy.​ Due to these advantageous properties, superalloys are the number one choice in the motorsport and automotive industries.

Lestercast have built up a strong relationship over the last 50 years with the Motorsport industry. We regularly attend meetings and support the MIA year on year with their Business Awards. We have gained a great network of customers throughout this industry and they have remained our customers for many years. We pride ourselves on achieving the highest quality investment cast components throughout the industry.

The investment casting manufacturing process used with rapid prototyping techniques, allows complex thin walled parts to be cast which may have been impossible with normal tooling methods.

We are an ISO9001:2015 & IATF 16949:2016 accredited metal casting company and are also JOSCAR registered.

For a full list of the types of metals that we cast and the particular grades, please visit our technical data page.

ADVANTAGES OF SUPERALLOY CASTINGS

HIGHLY RESISTANT TO CORROSION

HIGH STRENGTH

RESISTANT TO HIGH TEMPERATURES

HIGH QUALITY SURFACE FINISH

COMPLEX SHAPES

HIGHLY DURABLE

Types of Superalloys Available;

 

  • Inconel 625, Inconel 600 & Inconel 601
  • Hastelloy X, Hastelloy B, Hastelloy B2, Hastelloy C, Hastelloy D
  • ST 6, ST 8 & ST 31
  • Haynes C242
  • HS188

 

It is important to consider the use for the final end product when selecting the correct type and it’s forward usage.

Investment casting motorsport
Investment Casting A Three Port Collector for a Hyper Car…

OTHER PROPERTIES OF SUPERALLOYS TO CONSIDER;

HIGHER COST

REASONABLY DIFFICULT TO MACHINE

Industrial use of Superalloys

  • Motorsport
  • Chemical
  • Energy
  • Food machinery
  • Nuclear
  • Pharmaceutical
  • Railway
  • Sub-sea
Inconel Investment casting oil gas
Inconel Investment casting

The data is the table should be used for guidance only.

SPECIFICATION

CHARACTERISTICS & TYPICAL APPLICATIONS

INCONEL 625 (CW6MC)

Good casting alloy with excellent machining and bearing properties. Aero- and land-based turbine engine parts
Exhaust systems, fuel systems, rocket and space application components, chemical and process industry parts, oil well, petroleum and natural gas industry parts.

INCONEL 600

These products have been used typically for parts requiring oxidation resistance, but useful at the higher temperatures only when stresses are low, and where such parts may require welding during fabrication, but usage is not limited to such applications. Strength at elevated temperatures is similar to that of 18-8 type steels.

INCONEL 601

Heat treating baskets and fixtures, radiant furnace tubes, strand - annealing tubes, thermocouple protection tubes, and furnace muffles and retorts. Thermal reactors for controling automotive emissions.

HASTELLOY X

Exceptional oxidation resistance. Highly resistant to stress corrosion cracking in petrochemical applications.
Gas turbine engines; Industrial furnaces; Chemical processing; Petrochemical processing.

HASTELLOY B

Used typically for parts, such as exducers and fans, requiring good corrosion resistance and strength, usage is not limited to such applications.Gas turbine bolting and shafting.

HASTELLOY C

Primarily for parts and assemblies, such as turbine rotors, shafts, blades, and bolts, requiring high strength up to 1500°F (816°C) and oxidation resistance up to 2000°F (1093°C).

HASTELLOY D / ANC 17

Good corrosion resistance, particulary when used with hot sulphric acid. Used in chemical plant components.

ST 6

Hard alloy, very wear resistant at high temperatures. General-purpose wear resistance applications. Valve seats and gates, pump shafts and bearings, erosion shields and rolling couples.

ST 8 / ANC 14

High strength and heat resistant alloy. Good resistance to oxidation and corrosion at high temperatures. Typical applications are impellers, gas turbines, valves at high service temperatures.

ST 31

A cobalt base superalloy with high wear and corrosion resistance, excellent stress-rupture properties, resistance to thermal and mechanical shock and corrosion resistance. It is commonly used in the hottest sections of industrial gas turbines.

C242 HAYNES / ANC11

Medium strength alloy, excellent resistance to oxidation and thermal fatigue at temperatures over 1000°C. Good thermal shock resistance upto 1100°C. Typical application is Gas turbine stator blades.

HS188